Ferranadium - bu taxminan 35% dan 85% temir va vanadiyning qotishmasi. Ferrandium asosan avtomobillar, qurilish konstruktsiyalari va tibbiy asbob-uskunalar uchun po'lat ishlab chiqarishda asosiy qo'shimcha sifatida ishlatiladi.
Ferro vanadiy

Ferranadium parametrlari
| Baho | Ichida | Aldamoq | n | Si | Bilan |
| Fev40-a | 38-45 | 1.5 | 0.09 | 2 | 0.6 |
| Fev40-b | 38-45 | 2 | 0.15 | 3 | 0.8 |
| Fev50-a | 48-55 | 1.5 | 0.07 | 2 | 0.4 |
| Fev5- b | 45-55 | 2 | 0.1 | 2.5 | 0.6 |
| Fev60-a | 58.0 ~ 65.0 | 1.5 | 0.06 | 2 | 0.4 |
| Fev60 - b | 58.0 ~ 65.0 | 2 | 0.1 | 2.5 | 0.6 |
| Fev60-a | 58.0 ~ 65.0 | 0.4 | 2 | 0.06 | 0.04 |
| Fev60 - b | 58.0 ~ 65.0 | 0.6 | 2.5 | 0.1 | 0.05 |
| Fev80-a | 78-82 | 1.5 | 0.05 | 1.5 | 0.15 |
| Fev80-b | 78-82 | 2 | 0.06 | 1.5 | 0.2 |