Ferroxrom temir qotishmasi bo'lib, uning asosiy komponentlari sifatida xrom va temir mavjud. Bu po'lat sanoatida asosiy qotishma agentlaridan biridir. Ferroxrom tarkibida 50% dan 70% gacha xrom mavjud.
ferroxrom
Ferroxrom tasnifi
Baho | Kimyoviy tarkibi (%) | |||||
Cr | C | Si | P | S | ||
Mikro uglerod |
FeCr-1 | 58-68 | 0.03-0.15 | 1.0-2.0 | 0.03-0.06 | 0.025-0.03 |
FeCr-2 | 63-68 | 0.03-0.15 | 1.0-2.0 | 0.03-0.06 | 0.025-0.03 | |
Kam uglerod |
FeCr-3 | 58-68 | 0.25-0.5 | 1.5-3.0 | 0.03-0.06 | 0.025-0.03 |
FeCr-4 | 63-68 | 0.25-0.5 | 1.5-3.0 | 0.03-0.06 | 0.025-0.03 | |
O'rtacha uglerod |
FeCr-5 | 58-68 | 1.0-4.0 | 1.5-3.0 | 0.03-0.06 | 0.025-0.03 |
FeCr-6 | 63-68 | 1.0-4.0 | 1.5-3.0 | 0.03-0.06 | 0.025-0.03 | |
Yuqori uglerod |
FeCr-7 | 58-68 | 4.0-10.0 | 3.0-5.0 | 0.03-0.06 | 0.03-0.06 |
FeCr-8 | 63-68 | 4.0-10.0 | 3.0-5.0 | 0.03-0.06 | 0.03-0.06 |
Zhen'an Metallurgy Xitoyda yuqori sifatli, raqobatbardosh narxlar va yuqori obro'ga ega bo'lgan professional metallurgiya mahsulotlarini yetkazib beruvchi hisoblanadi. Fabrikamıza tashrif buyurishga xush kelibsiz.