50 Ferro Vanadium Description
Two types of ferrovanadium are commonly used, containing 50% and 80% vanadium. FeV50 is suitable for vanadium-containing grades and are added to steel in the same way. FeV50 has a higher melting point, it is suitable for both BOF and EAF applications because the ferrovanadium dissolves in the steel.
50 Ferrovanadium: V 48.0%-55.0%,Si 2.0%-2.5%,Al 1.5%-2.0%,C 0.4%-0.6%,P 0.06%-0.10%,S 0.04%-0.05%
![]()
50 Ferro Vanadium Composition
| Ferro Vandadium 50 composition (%) | |||||
| V | P | C | |||
| FeV50-A | 48-55 | 1.5 | 0.07 | 2 | 0.4 |
| FeV50-B | 45-55 | 2 | 0.1 | 2.5 | 0.6 |
| 10-50mm | |||||
| 60-325mesh | |||||
| 80-270mesh & customize size | |||||
Our products have been exported to more than 100 countries and regions such as Japan, South Korea, Southeast Asia, USA, Brazil and Europe. Its good quality, competitive price, timely delivery and best after-sales service are highly appreciated by our customers.
![]()
![]()
A: Yes, we have it in stock. The exact delivery time depends on your detailed quantity and is usually around 7-15 days.
Issiq teglar: 50 ferro vanadium lumps, China 50 ferro vanadium lumps manufacturers, suppliers