Qisqartma:fesi 75
Hajmi: 10-50mm, 50-100mm, moslashtirilishi mumkin
Shakli: bo'lak, kukun, to'p
Batafsil parametrlar:si 75 dan katta yoki teng
Foydalanish: deoksidlanish, po'lat ishlab chiqarish, quyish va boshqalar.
Ferrosilikon 75

Ferrosilikon 75 tarkibiy qismlari
| Model | Kimyoviy tarkibi (%) | |||||
| Si | Mn | Al | C | P | S | |
| FeSi75A | 75.0-80.0 | 0 dan kichik yoki unga teng.4 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.2 | 0 dan kichik yoki unga teng.035 | 0 dan kichik yoki unga teng.02 |
| FeSi75B | 73.0-80.0 | 0 dan kichik yoki unga teng.4 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.2 | 0 dan kichik yoki unga teng.04 | 0 dan kichik yoki unga teng.02 |
| FeSi75C | 72.0-75.0 | 0 dan kichik yoki unga teng.5 | 2 dan kichik yoki teng.0 | 0 dan kichik yoki unga teng.1 | 0 dan kichik yoki unga teng.04 | 0 dan kichik yoki unga teng.02 |