Umumiy qadoqlash va metall kremniy kukunining o'lchamlari

Apr 10, 2024 Xabar QOLDIRISH

Metall kremniy kukunispetsifikatsiyalar va zarrachalar o'lchamlari: 60 mesh, 100 mesh, 300 mesh, 150-600 mesh, eng keng tarqalgani 325 mesh bo'lib, u ham mijozlar talablariga muvofiq sozlanishi mumkin.
Metall silikon kukunli qadoqlash: tonna sumkalar (1000kg / sumka) yoki mijozlar talablariga muvofiq tayyorlangan

Metall kremniy kukuni

silicon metal powder


Metall kremniy kukuni tarkibi

Silikon kukuni Hajmi

(to'r)
Kimyoviy tarkibi %
Si Fe Al Ca
dan katta yoki teng dan kichik yoki teng
Kimyoviy
kremniy kukuni
Si-(20-100 mesh)
Si-(30-120 mesh)
Si-(40-160 mesh)
Si-(100-200 mesh)
Si-(45-325 mesh)
Si-(50-500 mesh)
99.6 0.2 0.15 0.05
99.2 0.4 0.2 0.1
99.0 0.4 0.4 0.2
98.5 0.5 0.5 0.3
98.0 0.6 0.5 0.3
O'tga chidamli kremniy kukuni -150 tarmoq
-200 tarmoq
-325 tarmoq
-400 tarmoq
-600mesh
99.6 0.2 0.15 0.05
99.2 0.4 0.2 0.1
99.0 0.4 0.4 0.2
98.5 0.5 0.3 0.2
98.0 0.6 0.5 0.3
Past darajali -200 tarmoq
-325 tarmoq
95-97 Nopoklik 3 dan kam yoki unga teng.0%

 

Kompaniyamiz ishlab chiqarish, sotish va sotishdan keyingi xizmat ko'rsatish uchun o'z SOP tizimiga ega. Umid qilamanki, biz sizga yaxshi va professional xizmatlarni taqdim eta olamiz!